Antibacterial AgNPs/CaP biocomposites / A. A. Ivanova [et al.]
Язык: английский.Серия: Advanced Material & Nanotechnology • PosterРезюме или реферат: The modification of implant surface is in the focus of many scientists worldwide. In this study, multifunctional biocomposite on the basis of calcium phosphate coating and silver nanoparticles has been fabricated through the use of nanofabrication techniques. Dense nanocrystalline HA film was deposited over AgNPs. The properties as well as the in vitro behavior of the developed biocomposites have been studied. The diffraction patterns of the biocomposites revealed the peaks of crystalline HA and silver (Ag). The release of Ag from the developed biocomposites was evaluated. The concentration of the released silver ions for 7 days of dissolution was 0.27±0.02 [mu]g/mL and 0.54±0.02 [mu]g/mL for phosphate and acetate buffers, respectively. In order to estimate the cytotoxicity of the samples the functional activity of osteoclasts, in particular, cell morphology, multinuclearity, actin ring and resorption pit on the substrates coated with HA and AgNPs-HA have been evaluated..Примечания о наличии в документе библиографии/указателя: [References: 12 tit.].Тематика: электронный ресурс | труды учёных ТПУ | тонкие пленки | гидроксиапатит | многослойные структуры | наночастицы | серебро | магнетронное распыление Ресурсы он-лайн:Щелкните здесь для доступа в онлайнTitle screen
[References: 12 tit.]
The modification of implant surface is in the focus of many scientists worldwide. In this study, multifunctional biocomposite on the basis of calcium phosphate coating and silver nanoparticles has been fabricated through the use of nanofabrication techniques. Dense nanocrystalline HA film was deposited over AgNPs. The properties as well as the in vitro behavior of the developed biocomposites have been studied. The diffraction patterns of the biocomposites revealed the peaks of crystalline HA and silver (Ag). The release of Ag from the developed biocomposites was evaluated. The concentration of the released silver ions for 7 days of dissolution was 0.27±0.02 [mu]g/mL and 0.54±0.02 [mu]g/mL for phosphate and acetate buffers, respectively. In order to estimate the cytotoxicity of the samples the functional activity of osteoclasts, in particular, cell morphology, multinuclearity, actin ring and resorption pit on the substrates coated with HA and AgNPs-HA have been evaluated.
Adobe Reader
Для данного заглавия нет комментариев.