Features of chemical-mineralogical composition and processing properties for medium-ferrous bauxites / L. P. Govorova [et al.]
Уровень набора: (RuTPU)RU\TPU\network\4526, MATEC Web of ConferencesЯзык: английский.Резюме или реферат: The features of chemical-mineralogical composition and processing properties of bauxites from Iksinsk and Severoonezhsk deposits are investigated in the paper. It is found that the studied bauxites are coarsely dispersed and low-dispersive, high-alumina clay raw materials with a high content of colouring oxides. According to their mineralogical composition, Iksinsk and Severoonezhsk bauxites are boehmitehydrargillite-kaolinite clay bauxites. Moreover, Iksinsk bauxite samples are characterized by the total absence of quartz impurities. The samples of plastic molding based on Iksinsk bauxites are fully sintered at 1500 °С with the formation of strong structures with a compressive strength of 70- 120 MPa (depending on the variety of bauxites). The samples based on Severoonezhsk bauxites are fully sintered at 1450 °С, and they are characterized by a compressive strength to 70 MPa in the sintered state..Примечания о наличии в документе библиографии/указателя: [References: 4 tit.].Тематика: электронный ресурс | труды учёных ТПУ | химико-минералогический состав | технологические свойства | бокситы | глинистое сырье | пластмассы | примеси Ресурсы он-лайн:Щелкните здесь для доступа в онлайн | Щелкните здесь для доступа в онлайнTitle screen
[References: 4 tit.]
The features of chemical-mineralogical composition and processing properties of bauxites from Iksinsk and Severoonezhsk deposits are investigated in the paper. It is found that the studied bauxites are coarsely dispersed and low-dispersive, high-alumina clay raw materials with a high content of colouring oxides. According to their mineralogical composition, Iksinsk and Severoonezhsk bauxites are boehmitehydrargillite-kaolinite clay bauxites. Moreover, Iksinsk bauxite samples are characterized by the total absence of quartz impurities. The samples of plastic molding based on Iksinsk bauxites are fully sintered at 1500 °С with the formation of strong structures with a compressive strength of 70- 120 MPa (depending on the variety of bauxites). The samples based on Severoonezhsk bauxites are fully sintered at 1450 °С, and they are characterized by a compressive strength to 70 MPa in the sintered state.
Для данного заглавия нет комментариев.