Time-Keeping Factor at a Constant Temperature in the Process of Spark Plasma Sintering / A. A. Sivkov [et al.]

Уровень набора: Nanotechnologies in Russia = 2006-Альтернативный автор-лицо: Sivkov, A. A., Specialist in the field of electric power engineering, Professor of Tomsk Polytechnic University, Doctor of technical sciences, 1951-, Aleksandr Anatolyevich;Gerasimov, D. Yu., Specialist in the field of electric power engineering, Associate Professor of Tomsk Polytechnic University, Candidate of technical sciences, 1980-, Dmitry Yurievich;Ivashutenko, A. S., specialist in the field of electrical engineering, Head of the Department of the Tomsk Polytechnic University, Candidate of technical sciences, 1981-, Alexander Sergeevich;Evdokimov, A. A., Specialist in the field of electric power engineering, Laboratory assistant of Tomsk Polytechnic University, 1987-, Andrey AnatolievichКоллективный автор (вторичный): Национальный исследовательский Томский политехнический университет, Инженерная школа энергетики, Отделение электроэнергетики и электротехники (ОЭЭ)Язык: английский.Страна: .Резюме или реферат: The dependence of the effect of time delay at a constant maximum temperature on the physicomechanical parameters of the sintered sample has been considered. Based on the results of the work, it can be concluded that it is necessary to reduce the duration of all sections of the sintering process in order to exclude the recrystallization factor, which worsens the parameters of the ceramics..Примечания о наличии в документе библиографии/указателя: [References: p. 544 (12 tit.)].Аудитория: .Тематика: электронный ресурс | труды учёных ТПУ | спекание | рекристаллизация | керамика Ресурсы он-лайн:Щелкните здесь для доступа в онлайн
Тэги из этой библиотеки: Нет тэгов из этой библиотеки для этого заглавия. Авторизуйтесь, чтобы добавить теги.
Оценка
    Средний рейтинг: 0.0 (0 голосов)
Нет реальных экземпляров для этой записи

Title screen

[References: p. 544 (12 tit.)]

The dependence of the effect of time delay at a constant maximum temperature on the physicomechanical parameters of the sintered sample has been considered. Based on the results of the work, it can be concluded that it is necessary to reduce the duration of all sections of the sintering process in order to exclude the recrystallization factor, which worsens the parameters of the ceramics.

Для данного заглавия нет комментариев.

оставить комментарий.