Effect of Mechanical Load on Defects Level in Soft Ferrite Ceramics / A. B. Petrova, A. V. Malyshev, A. P. Surzhikov
Уровень набора: (RuTPU)RU\TPU\network\7958, European Physical Journal Web of Conferences (EPJ Web of Conferences)Язык: английский.Страна: France.Резюме или реферат: The article presents the results of a study of the effect of mechanical load on the temperature dependence of the initial permeability of LiTiZn soft ferrite ceramics. Regimes of mechanical load were created by a steel non-magnetic ring with screws. In this work, four levels of mechanical load were investigated: without load, with 1, 2 and 3 screws. For obtaining temperature dependences and exclude the influence of prehistory on the initial permeability, the samples were heated to a temperature exceeding the Curie point by 50 degrees, after which they slowly cooled to room temperature. The defects level was determined by the ratio of the parameters ? / ? of the phenomenological expression, which describes the experimental temperature dependences. It is shown that as the mechanical load increases, the defects level of ferrite ceramics increases, and after load removing, it returns to its original level..Примечания о наличии в документе библиографии/указателя: [References: 11 tit.].Тематика: электронный ресурс | труды учёных ТПУ | механические нагрузки | ферритовая керамика | температурные зависимости Ресурсы он-лайн:Щелкните здесь для доступа в онлайн | Щелкните здесь для доступа в онлайнTitle screen
[References: 11 tit.]
The article presents the results of a study of the effect of mechanical load on the temperature dependence of the initial permeability of LiTiZn soft ferrite ceramics. Regimes of mechanical load were created by a steel non-magnetic ring with screws. In this work, four levels of mechanical load were investigated: without load, with 1, 2 and 3 screws. For obtaining temperature dependences and exclude the influence of prehistory on the initial permeability, the samples were heated to a temperature exceeding the Curie point by 50 degrees, after which they slowly cooled to room temperature. The defects level was determined by the ratio of the parameters ? / ? of the phenomenological expression, which describes the experimental temperature dependences. It is shown that as the mechanical load increases, the defects level of ferrite ceramics increases, and after load removing, it returns to its original level.
Для данного заглавия нет комментариев.