The Hydrothermal Synthesis Duration Influence on Calcium Phosphate and Hydroxyapatite Phase Composition / K. Chuprunov, A. Yudin, D. Leybo [et al.]
Уровень набора: (RuTPU)RU\TPU\network\2008, IOP Conference Series: Materials Science and EngineeringЯзык: английский.Страна: .Резюме или реферат: This paper reports the hydrothermal synthesis process duration influence on phase composition, crystallinity degree, morphology and dispersity of the hydroxyapatite powder. The calcium phosphate and hydroxyapatite were synthesized in precursor system Ca(NO[3])[2](NH[4])[2]HPO[4]-NH[4]OH. The obtained powders were characterized with X-Ray diffraction, Fourier Transform spectroscopy (FTIR) and Raman spectroscopy. The results demonstrate: the increasing of the synthesis time duration has no influence on the phase composition. However, the synthesis duration time growth from 12 to 48 hours make possible increase the crystallinity degree from 0.68 to 0.98..Примечания о наличии в документе библиографии/указателя: [References: 23 tit.].Тематика: электронный ресурс | труды учёных ТПУ | гидротермальный синтез | фазовый состав | фосфат кальция | гидроксиапатиты | кристалличность | морфология | дисперсность | порошки | рентгеновская дифракция | спектроскопия | Фурье-преобразования | комбинационное рассеяние | синтез Ресурсы он-лайн:Щелкните здесь для доступа в онлайн | Щелкните здесь для доступа в онлайнTitle screen
[References: 23 tit.]
This paper reports the hydrothermal synthesis process duration influence on phase composition, crystallinity degree, morphology and dispersity of the hydroxyapatite powder. The calcium phosphate and hydroxyapatite were synthesized in precursor system Ca(NO[3])[2](NH[4])[2]HPO[4]-NH[4]OH. The obtained powders were characterized with X-Ray diffraction, Fourier Transform spectroscopy (FTIR) and Raman spectroscopy. The results demonstrate: the increasing of the synthesis time duration has no influence on the phase composition. However, the synthesis duration time growth from 12 to 48 hours make possible increase the crystallinity degree from 0.68 to 0.98.
Для данного заглавия нет комментариев.