Conditions for Quality Dimensions in Direct Laser Melting of Copper / N. A. Saprykina, A. A. Saprykin, E. A. Ibragimov, A. A. Saprykin
Уровень набора: (RuTPU)RU\TPU\network\11477, Key Engineering Materials, Scientific JournalЯзык: английский.Резюме или реферат: This paper analyzes the effect of SLM parameters on mechanical characteristics and surface roughness of a single-component copper powder. The study reports on appropriate SLM conditions for a single-component copper powder; to form a layer a technique within layer-by-layer selective laser melting is suggested and comprises roughing, semi-finishing and finishing modes. The work establishes a range to vary surface roughness, porosity and ultimate compressive strength of a single-component copper powder by means of laser processing conditions. Rz is variable 332 to 689 ?m, porosity ranges approximately 13-39%, and ultimate compressive strength is 8 to 104 МPа..Аудитория: .Тематика: электронный ресурс | труды учёных ТПУ | coagulation | copper | melting conditions | porosity | quality | roughness | Selective Laser Melting (SLM) | ultimate compressive strength | коагуляция | медь | плавление | пористость | прочность Ресурсы он-лайн:Щелкните здесь для доступа в онлайнНет реальных экземпляров для этой записи
Title screen
This paper analyzes the effect of SLM parameters on mechanical characteristics and surface roughness of a single-component copper powder. The study reports on appropriate SLM conditions for a single-component copper powder; to form a layer a technique within layer-by-layer selective laser melting is suggested and comprises roughing, semi-finishing and finishing modes. The work establishes a range to vary surface roughness, porosity and ultimate compressive strength of a single-component copper powder by means of laser processing conditions. Rz is variable 332 to 689 ?m, porosity ranges approximately 13-39%, and ultimate compressive strength is 8 to 104 МPа.
Для данного заглавия нет комментариев.
Личный кабинет оставить комментарий.