200 1 _aEffect of the passivating coating type, particle size, and storage time on oxidation and nitridation of aluminum powders
_fA. A. Gromov [et al.]
203 _aText
_celectronic
300 _aTitle screen
320 _a[References: p. 184 (14 tit.)]
330 _aProcesses of nonisothermal oxidation, nitridation, and ageing of aluminum powders with different particle sizes (nano-sized powder, ASD-1 powder, and PAP-2 powder) are considered. Application of non-oxide coatings onto particles of aluminum nanopowders reduces their thermal stability. Owing to scale-shaped particles, the PAP-2 powder after long-time storage preserves high activity of oxidation and nitridation, which is commensurable with that of the aluminum nanopowder. The activity of the coarse ASD-1 powder consisting of spherical particles in terms of oxidation and nitridation is low and only slightly changes during ageing.
333 _aРежим доступа: по договору с организацией-держателем ресурса
461 _tCombustion, Explosion and Shock Waves
_d1965-
463 _tVol. 42, № 2
_v[P. 177-184]
_d2006
610 1 _aэлектронный ресурс
610 1 _aтруды учёных ТПУ
610 1 _aaluminum powders
610 1 _anon-oxide coatings
610 1 _aoxidation
610 1 _aageing
610 1 _anitridation
610 1 _aair
701 1 _aGromov
_bA. A.
_cChemical Engineer
_cProfessor of Tomsk Polytechnic University, Doctor of technical sciences
_f1975-
_gAleksandr Aleksandrovich
_2stltpush
_3(RuTPU)RU\TPU\pers\33059
701 1 _aIlyin
_bA. P.
_cchemist
_cProfessor of Tomsk Polytechnic University, Doctor of physical and mathematical sciences
_f1949-
_gAleksandr Petrovich
_2stltpush
_3(RuTPU)RU\TPU\pers\33060
701 1 _aFoerter-Barth
_bU.
701 1 _aTeipel
_bU.
801 2 _aRU
_b63413507
_c20160830
_gRCR
856 4 _uhttp://dx.doi.org/10.1007/s10573-006-0036-4
942 _cCF