000 | 03166nla2a2200433 4500 | ||
---|---|---|---|
001 | 650381 | ||
005 | 20231030040943.0 | ||
035 | _a(RuTPU)RU\TPU\network\15599 | ||
035 | _aRU\TPU\network\15598 | ||
090 | _a650381 | ||
100 | _a20161004a2016 k y0engy50 ba | ||
101 | 0 | _aeng | |
102 | _aGB | ||
105 | _ay z 100zy | ||
135 | _adrgn ---uucaa | ||
181 | 0 | _ai | |
182 | 0 | _ab | |
200 | 1 |
_aEnhancing the Lifetime of Welded Joints Using the Protective Coating and Causes the Formation of Defects in Them _fV. P. Bezborodov, Yu. N. Saraev |
|
203 |
_aText _celectronic |
||
300 | _aTitle screen | ||
320 | _a[References: 14 tit.] | ||
330 | _aThe paper shows the efficacy of eutectic Nickel coatings for protecting welded joints of steels against corrosion. It increases with increasing content of the eutectic and chemical compounds at the grain boundaries γ-solid solution based on Nickel. Refinement of the structure of the coatings and reduce their heterogeneity allows to increase the protective properties and durability of welded joints against corrosion. It is established that the probability of formation of cracks in the coatings increases with their thickness, intensity of heating and cooling after reflow, and also with increasing content of the eutectic and chemical compounds at the grain boundaries γ-solid solution based on Nickel. Shown to prevent the formation of cracks in the coatings when they are melt you can use optimal modes of heating and cooling of the composition. Modification of the structure of the coatings by grinding them and reducing heterogeneity allows to improve the resistance to crack formation and protective properties of welded joints. | ||
461 | 0 |
_0(RuTPU)RU\TPU\network\2008 _tIOP Conference Series: Materials Science and Engineering |
|
463 | 0 |
_0(RuTPU)RU\TPU\network\15319 _tVol. 142 : Innovative Technologies in Engineering _oVII International Scientific Practical Conference, 19–21 May 2016, Yurga, Russian Federation _o[proceedings] _v[012023, 7 p.] _d2016 |
|
610 | 1 | _aэлектронный ресурс | |
610 | 1 | _aтруды учёных ТПУ | |
610 | 1 | _aжизненный цикл | |
610 | 1 | _aсварные соединения | |
610 | 1 | _aзащитные покрытия | |
610 | 1 | _aдефекты | |
610 | 1 | _aникель | |
610 | 1 | _aкоррозия | |
700 | 1 |
_aBezborodov _bV. P. _cspecialist in the field of materials science _cassociate Professor of Tomsk Polytechnic University, candidate of technical Sciences _f1955- _gValery Pavlovich _2stltpush _3(RuTPU)RU\TPU\pers\33543 |
|
701 | 1 |
_aSaraev _bYu. N. |
|
712 | 0 | 2 |
_aНациональный исследовательский Томский политехнический университет (ТПУ) _bИнститут физики высоких технологий (ИФВТ) _bКафедра материаловедения и технологии металлов (МТМ) _h73 _2stltpush _3(RuTPU)RU\TPU\col\18689 |
801 | 2 |
_aRU _b63413507 _c20170120 _gRCR |
|
856 | 4 | _uhttp://dx.doi.org/10.1088/1757-899X/142/1/012023 | |
856 | 4 | _uhttp://earchive.tpu.ru/handle/11683/34707 | |
942 | _cCF |